Customization: | Available |
---|---|
Shape: | Powder |
Application: | Industrial |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Features
Cobalt-chromium-tungsten alloy is not strengthened by the ordered precipitated phase firmly bound to the matrix, but by the austenitic fcc matrix and a small number of carbides distributed in the matrix.
High strength when folded at high temperature.
Carbide strengthening phase.
The strength of folded alloy decreases slowly.
Good thermal corrosion resistance.
Main chemical composition | |
Co: ≥ 60.5 | Cr: 26.0-28.0 |
W: 7.5-10.00 | Si: 0.5-1.5 |
main products |
CoCrW |
|||
Main grain size range |
0-25 μm |
15-53 μm |
45-105 μm |
75-150 μm |
mobility |
15-53μm |
≤20s/50g |
||
Bulk density |
≥4.50/cm3 |
|||
oxygen content |
≤300ppm |
|||
nitrogen content |
≤300ppm |
|||
mechanical property |
compressive strength /MPa 1000±50 yield strength /MPa 800±50 Elongation /% 30±2 |